Roslag: norwegische Weise Holz von Nässe beschützen: Difference between revisions

From EduFarm
Content deleted Content added
Nils (talk | contribs)
m English Struktur
Nils (talk | contribs)
Line 1: Line 1:
== 1.Composition and application ==
== 1.Composition and Application ==

=== Composition ===
(1/3) Pine tar (Norwegian tar), (1/3) turpentine oil, and (1/3) linseed oil

=== Application ===
Initially 2 to 3 coats on dry wood (light layer), then 4 to 5 coats on wet wood to fully saturate the wood fibers.


== 2.Risks of degassing ==
== 2.Risks of degassing ==

Revision as of 14:23, 24 June 2026

1.Composition and Application

Composition

(1/3) Pine tar (Norwegian tar), (1/3) turpentine oil, and (1/3) linseed oil

Application

Initially 2 to 3 coats on dry wood (light layer), then 4 to 5 coats on wet wood to fully saturate the wood fibers.

2.Risks of degassing